grs creativity engraving
See more: Metalworking
Materials:
- QC Onglette
- 38 Flat
- Brass wire for punch
- .61 mm Copper wire
Shaping the QC Onglette
| Post | Tilt | Beg Grit | End Grit | |
|---|---|---|---|---|
| 1 | 55 | Face | 260 | Ceramic |
Shaping the 38 Flat
| Post | Tilt | Beg Grit | End Grit | |
|---|---|---|---|---|
| 1 | 45 | Face | 260 | 1200 |
| 2 | 2.5 | 0 | 260 | |
| 3 - HEEL | 20 | 0 | 1200 | Ceramic |
Making the punch
| Post | Tilt | Beg Grit | End Grit | |
|---|---|---|---|---|
| 1 | 90 | 90 | 180 | 180 |
To note
- Graver is width of the wire
- Punch is twice the width of the wire
- Grave here and here with the flat graver

- Connect points. Takes a couple passes to get to the depth you need.
- Take annealed copper wire. Make sure that the wire is half in the hole.

- Drag graver against the walls.

- With onglette make thorns in metal. Don’t be surprised if onglette breaks, it’s fragile

- Flatten wire ends with file
- Punch the wire in the channel. One spot at a time.
- Then go back and go over it with the pusher
- Sand